Description: Zirconia is a bio-inert material. Since its application as an inorganic biomaterial in the 1970s, it has good biocompatibility, excellent corrosion resistance and wear resistance, stable chemical properties and good thermoelectric insulation. Such biological properties, especially the aesthetic effects closest to natural teeth, are gradually being applied in the field of stomatology. Application: This product can be used as a preparation for zirconia ceramics, and has been widely used in the repair of dental defects and defects. This product can be mixed with other bioceramic materials, such as hydroxyapatite, ß-tricalcium phosphate, calcium silicate and other powders to enhance its biological activity. Information provided by Matexcel |