MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Stratasys® PC-ABS
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC-ABS is a blend of polycarbonate (PC) and acrylonitrile butadiene styrene (ABS) thermoplastics. The result is an FDM filament that exhibits optimal characteristics of each – excellent strength, high toughness and heat resistance, and good flexural strength. PC-ABS exhibits the strength of PC but the impact resistance of ABS. PC-ABS is suitable for a variety of applications that include prototyping, tooling and low-volume production. Available colors are black and white.

Information provided by Stratasys®

Vendors:
Available Properties
  • Specific Gravity, ASTM D257, XY, XZ/ZX Orientations
  • Tensile Strength at Break, ASTM D638, ZX Orientation
  • Tensile Strength at Break, ASTM D638, XZ Orientation
  • Tensile Strength, Yield, ASTM D638, XZ Orientation
  • Elongation at Break, ASTM D638, ZX Orientation
  • Elongation at Break, ASTM D638, XZ Orientation
  • Elongation at Yield, ASTM D638, XZ Orientation
  • Modulus of Elasticity, ASTM D638, ZX Orientation
  • Modulus of Elasticity, ASTM D638, XZ Orientation
  • Flexural Strength, ASTM D790, Procedure A, ZX Orientation
  • Flexural Modulus, ASTM D790, Procedure A, ZX Orientation
  • Flexural Modulus, ASTM D790, Procedure A, XZ Orientation
  • Flexural Strain at Break, ASTM D790, Procedure A, ZX Orientation
  • Compressive Yield Strength, ASTM D695, XZ Orientation
  • Compressive Yield Strength, ASTM D695, ZX Orientation
  • Compressive Modulus, ASTM D695, XZ Orientation
  • Compressive Modulus, ASTM D695, ZX Orientation
  • Izod Impact, Notched, ASTM D256, ASTM D4812, ZX Orientation
  • Izod Impact, Notched, ASTM D256, ASTM D4812, XZ Orientation
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, ZX Orientation
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, XZ Orientation
  • Volume Resistivity, ASTM D257, XY, XZ/ZX Orientations
  • Dielectric Constant, ASTM D150, XY Orientation
  • Dielectric Constant, ASTM D150, XY Orientation
  • Dielectric Constant, ASTM D150, XZ/ZX Orientation
  • Dielectric Constant, ASTM D150, XZ/ZX Orientation
  • Dissipation Factor, ASTM D150, XY Orientation
  • Dissipation Factor, ASTM D150, XZ/ZX Orientation
  • Dissipation Factor, ASTM D150, XY Orientation
  • Dissipation Factor, ASTM D150, XZ/ZX Orientation
  • CTE, linear, ASTM E831, XY Orientation
  • CTE, linear, ASTM E831, XY Orientation
  • CTE, linear, ASTM E831, XY Orientation
  • CTE, linear, ASTM E831, XZ/ZX Orientation
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648 Method B, XY, XZ/ZX Orientations
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648 Method B, XY, XZ/ZX Orientations
  • Glass Transition Temp, Tg, ASTM D7426, Inflection Point, XY, XZ/ZX
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.