MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
C.O.I.M. FILCO® 658 N Non Ionic Aqueous Emulsion of Unsaturated Polyester Polymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Description: Non Ionic Aqueous Emulsion of Unsaturated Polyester Polymer
General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.
Applications: Filco 658 N has been studied as an insoluble binder for glass fiber. Particularly for chopped strand mat, continuous strand mat and perform.
It is also suggested as a film forming component of glass fiber sizing for SMC, BMC, and DMC.
When Filco 658 N is used as an insoluble liquid binder benzoyl peroxide must be added (0.6 - 1.2% of active peroxide on Filco 658 N). Temperatures between 160°C and 190°C for 40 - 60 seconds are recommended for the binder cross link in the dryers during the mat production process.
When Filco 658 N is used as a film former in glass fiber sizing formulations for SMC, BMC, and DMC no benzoyl peroxide should be added.
In both applications the resulting products make thermosetting glass/resin composites having good physical and mechanical properties.
Information provided by P.A.T. Products, Inc.

Vendors:
Available Properties
  • Solids Content
  • Particle Size, MA147LFE
  • pH, MA148LFE
  • Brookfield Viscosity, Brookfield RVT spindle 2.2 RPM
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
C.O.I.M. S.p.A.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.