Overview of materials for Epoxy/Carbon Fiber Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 2.25 g/cc0.0415 - 0.0813 lb/in³Average value: 1.42 g/cc Grade Count:96
Filler Content 40.0 - 62.0 %40.0 - 62.0 %Average value: 55.1 % Grade Count:66
Water Absorption 0.0500 - 3.90 %0.0500 - 3.90 %Average value: 2.16 % Grade Count:4
Moisture Absorption at Equilibrium <= 1.00 %
@Temperature 71.1 - 71.1 °C
<= 1.00 %
@Temperature 160 - 160 °F
Average value: 1.00 % Grade Count:2
Viscosity 25000 - 450000 cP25000 - 450000 cPAverage value: 242000 cP Grade Count:6
 2000 - 100000 cP
@Temperature 60.0 - 150 °C
2000 - 100000 cP
@Temperature 140 - 302 °F
Average value: 27000 cP Grade Count:12
Linear Mold Shrinkage 0.000 - 0.00110 cm/cm0.000 - 0.00110 in/inAverage value: 0.000488 cm/cm Grade Count:17
Outgassing - Total Mass Loss 0.240 - 0.700 %0.240 - 0.700 %Average value: 0.420 % Grade Count:11
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 60.0 - 65.060.0 - 65.0Average value: 63.3 Grade Count:3
Hardness, Shore D 85.0 - 90.085.0 - 90.0Average value: 88.3 Grade Count:3
Tensile Strength, Ultimate 0.917 - 4140 MPa133 - 600000 psiAverage value: 965 MPa Grade Count:139
 4.37128 - 3013.01 MPa
@Temperature -73.0 - 177 °C
634.001 - 437001 psi
@Temperature -99.4 - 351 °F
Average value: 1040 MPa Grade Count:41
Tensile Strength, Yield 4.62 - 3380 MPa670 - 490000 psiAverage value: 1260 MPa Grade Count:48
 2.965 - 2137 MPa
@Temperature -59.0 - 177 °C
430.0 - 309900 psi
@Temperature -74.2 - 351 °F
Average value: 945 MPa Grade Count:19
Elongation at Break 0.430 - 11.0 %0.430 - 11.0 %Average value: 1.52 % Grade Count:30
 0.500 - 1.72 %
@Temperature -55.0 - 93.3 °C
0.500 - 1.72 %
@Temperature -67.0 - 200 °F
Average value: 1.24 % Grade Count:5
Modulus of Elasticity 2.62 - 520 GPa380 - 75400 ksiAverage value: 101 GPa Grade Count:184
 4.74 - 323 GPa
@Temperature -73.0 - 177 °C
687 - 46800 ksi
@Temperature -99.4 - 351 °F
Average value: 96.2 GPa Grade Count:58
Flexural Yield Strength 22.6 - 2050 MPa3280 - 298000 psiAverage value: 973 MPa Grade Count:106
 399.896 - 4750.49 MPa
@Temperature -55.0 - 177 °C
58000.1 - 689001 psi
@Temperature -67.0 - 351 °F
Average value: 1010 MPa Grade Count:31
Flexural Modulus 3.38 - 638 GPa490 - 92500 ksiAverage value: 98.8 GPa Grade Count:106
 37.0 - 285 GPa
@Temperature -55.0 - 177 °C
5370 - 41300 ksi
@Temperature -67.0 - 351 °F
Average value: 98.0 GPa Grade Count:30
Compressive Yield Strength 6.63 - 1880 MPa962 - 273000 psiAverage value: 758 MPa Grade Count:155
 93.9 - 1862 MPa
@Temperature -73.0 - 177 °C
13600 - 270100 psi
@Temperature -99.4 - 351 °F
Average value: 705 MPa Grade Count:74
Compressive Modulus 0.0111 - 305 GPa1.61 - 44200 ksiAverage value: 77.2 GPa Grade Count:108
 5.75 - 285 GPa
@Temperature -73.0 - 177 °C
834 - 41300 ksi
@Temperature -99.4 - 351 °F
Average value: 86.3 GPa Grade Count:52
Ultimate Bearing Strength 965 - 1240 MPa140000 - 180000 psiAverage value: 1090 MPa Grade Count:3
Bearing Yield Strength 1.00 - 848 MPa145 - 123000 psiAverage value: 445 MPa Grade Count:5
Poissons Ratio 0.0200 - 0.9500.0200 - 0.950Average value: 0.286 Grade Count:15
 0.0240 - 0.960
@Temperature -73.0 - 177 °C
0.0240 - 0.960
@Temperature -99.4 - 351 °F
Average value: 0.462 Grade Count:6
Shear Modulus 1.93 - 5.60 GPa280 - 812 ksiAverage value: 4.02 GPa Grade Count:41
 0.700 - 5.72 GPa
@Temperature -70.0 - 177 °C
102 - 830 ksi
@Temperature -94.0 - 351 °F
Average value: 3.16 GPa Grade Count:20
Shear Strength 6.89 - 590 MPa1000 - 85600 psiAverage value: 89.8 MPa Grade Count:141
 26.2 - 164.095 MPa
@Temperature -73.0 - 177 °C
3800 - 23800.0 psi
@Temperature -99.4 - 351 °F
Average value: 66.5 MPa Grade Count:60
Izod Impact, Notched 8.00 - 15.0 J/cm15.0 - 28.1 ft-lb/inAverage value: 10.4 J/cm Grade Count:4
Tensile Impact Strength 12.0 - 90.0 kJ/m²5.71 - 42.8 ft-lb/in²Average value: 48.8 kJ/m² Grade Count:13
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.30e+13 ohm-cm100 - 1.30e+13 ohm-cmAverage value: 1.00e+12 ohm-cm Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear -0.700 - 186 µm/m-°C-0.389 - 103 µin/in-°FAverage value: 21.3 µm/m-°C Grade Count:15
CTE, linear, Transverse to Flow 2.10 - 225 µm/m-°C1.17 - 125 µin/in-°FAverage value: 67.6 µm/m-°C Grade Count:4
Specific Heat Capacity 1.00 - 1.20 J/g-°C0.239 - 0.287 BTU/lb-°FAverage value: 1.13 J/g-°C Grade Count:3
Thermal Conductivity 0.220 - 400 W/m-K1.53 - 2780 BTU-in/hr-ft²-°FAverage value: 78.8 W/m-K Grade Count:12
Maximum Service Temperature, Air 71.0 - 300 °C160 - 572 °FAverage value: 127 °C Grade Count:69
Minimum Service Temperature, Air -59.0 - 10.0 °C-74.2 - 50.0 °FAverage value: -22.2 °C Grade Count:6
Glass Transition Temp, Tg 45.0 - 370 °C113 - 698 °FAverage value: 154 °C Grade Count:70
Flammability, UL94 HB - V-0HB - V-0Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 5.00 - 180 °C41.0 - 356 °FAverage value: 134 °C Grade Count:69
Cure Time 5.00 - 1080 min0.0833 - 18.0 hourAverage value: 288 min Grade Count:8
 0.583333 - 4200 min
@Temperature 10.0 - 160 °C
0.00972222 - 70.0 hour
@Temperature 50.0 - 320 °F
Average value: 295 min Grade Count:24
Pot Life 45.0 - 75.0 min45.0 - 75.0 minAverage value: 69.0 min Grade Count:5
 0.500 - 225 min
@Temperature 10.0 - 138 °C
0.500 - 225 min
@Temperature 50.0 - 280 °F
Average value: 123 min Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.