Physical PropertiesMetricEnglishComments
Density 0.001553 g/cc0.00005611 lb/in³Gas
Molecular Weight 37.997 g/mol37.997 g/molF2
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 18.9984018.998401995
Atomic Number 99
X-ray Absorption Edge 17.913 Å17.913 ÅK
Critical Temperature -129.02 °C-200.24 °F
Electronegativity 3.983.98Pauling
Ionic Radius 0.0800 Å0.0800 ÅCrystal Ionic Radius for Valence +7
 1.33 Å1.33 ÅCrystal Ionic Radius for Valence -1
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 13.2 J/g5.68 BTU/lb
Specific Heat Capacity 0.824 J/g-°C0.197 BTU/lb-°Fat STP
Melting Point -219.66 °C-363.39 °F
Boiling Point -188.12 °C-306.62 °F
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 100 %100 %
 
Descriptive Properties
CAS Number7782-41-4

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.