Physical PropertiesMetricEnglishComments
Density 4.94 g/cc0.178 lb/in³theoretical
Molecular Weight 59.878 g/mol59.878 g/mol
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 2000 - 24002000 - 2400100 g load, single crystal
 2000 - 27502000 - 275050 g load, single crystal
 1800 - 59001800 - 5900
Hardness, Rockwell A 9393
Vickers Microhardness 32003200100 g load
Tensile Strength, Ultimate 258 MPa37400 psi
 59.0 MPa
@Temperature 1200 °C
8560 psi
@Temperature 2190 °F
 114 MPa
@Temperature 980 °C
16500 psi
@Temperature 1800 °F
Modulus of Elasticity 448 - 451 GPa65000 - 65400 ksi
Poissons Ratio 0.18 - 0.190.18 - 0.19at RT
Shear Modulus 110 - 193 GPa16000 - 28000 ksi
 186 GPa27000 ksisingle crystal
Shear Strength  89.0 MPa
@Temperature 1925 °C
12900 psi
@Temperature 3497 °F
 227 MPa
@Temperature 1600 °C
32900 psi
@Temperature 2910 °F
 757 - 2958 MPa
@Temperature 22.0 °C
110000 - 429000 psi
@Temperature 71.6 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000180 - 0.000250 ohm-cm0.000180 - 0.000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.70 µm/m-°C
@Temperature 20.0 °C
4.28 µin/in-°F
@Temperature 68.0 °F
Melting Point 3065 °C5549 °F
Solidus 3050 °C5520 °F
Liquidus 3080 °C5580 °F
 
Descriptive Properties
Crystal StructureCubicNaCl Structure
SolubilityInsoluble in H2O; Soluble in HNO3

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.