MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
VICTREX™ PEEK 450G™ General Purpose
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contact compliant, color natural/beige.

Typical Application Areas: Applications for higher strength and stiffness as well as high ductility. Chemically resistant to aggressive environments, suitable for sterilisation for medical and food contact applications.

Information provided by Victrex.

Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccCrystalline; ISO 1183
Water Absorption at Saturation 0.45 %
@Temperature 23.0 °C
ISO 62-1
 0.55 %
@Temperature 100 °C
ISO 62-1
Viscosity 350000 cP
@Temperature 400 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.013 cm/cm375°C nozzle, 190°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm375°C nozzle, 190°C tool; ISO 294-4
Spiral Flow 11.0 cm
@Thickness 1.00 mm
Mold Temp: 190°C, Melt Temp: 375°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84.5ISO 868
Tensile Strength, Yield 98.0 MPaISO 527
Elongation at Break 45 %ISO 527
Tensile Modulus 4.00 GPaISO 527
Flexural Strength 12.5 ksi
@Temperature 275 °C
ISO 178
 19.0 MPa
@Temperature 175 °C
ISO 178
 85.0 MPa
@Temperature 125 °C
ISO 178
 165 MPa
@Temperature 23.0 °C
ISO 178
 125 MPa
@Strain 3.5 %,
Temperature 23.0 °C
ISO 178
Flexural Modulus 3.80 GPaISO 178
Compressive Strength 70.0 MPa
@Temperature 120 °C
ISO 604
 125 MPa
@Temperature 23.0 °C
ISO 604
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180/U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/U
Charpy Impact, Notched 0.700 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cm
@Temperature 275 °C
IEC 60093
 1.00e+15 ohm-cm
@Temperature 125 °C
IEC 60093
 1.00e+16 ohm-cm
@Temperature 23.0 °C
IEC 60093
Dielectric Constant 3.0
@Frequency 50 Hz
IEC 60250
 3.1
@Frequency 1000 Hz
IEC 60250
 4.5
@Frequency 50 Hz,
Temperature 200 °C
IEC 60250
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
 200 kV/mm
@Thickness 0.500 mm
IEC 60243-1
Dissipation Factor 0.0040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
@Temperature <=143 °C
Below Tg; ISO 11359
 120 µm/m-°C
@Temperature >=143 °C
Above Tg; ISO 11359
CTE, linear, Transverse to Flow 55.0 µm/m-°C
@Temperature <=143 °C
Below Tg; ISO 11359
 140 µm/m-°C
@Temperature >=143 °C
Above Tg; ISO 11359
Thermal Conductivity 0.290 W/m-KAverage; ISO 22007-4
 0.350 W/m-KAlong flow; ISO 22007-4
Melting Point 343 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 152 °CAs molded; ISO 75-f
 160 °C
@Treatment Temp. 200 °C,
Time 14400 sec
Annealed; ISO 75-f
Glass Transition Temp, Tg 143 °COnset; ISO 11357
 150 °CMidpoint; ISO 11357
UL RTI, Electrical 260 °CUL 746B
UL RTI, Mechanical with Impact 180 °CUL 746B
UL RTI, Mechanical without Impact 240 °CUL 746B
Glow Wire Flammability Index 960 °C2 mm; IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 100 °CHopper
Rear Barrel Temperature 355 °C
Middle Barrel Temperature 360 - 365 °C
Front Barrel Temperature 370 °C
Nozzle Temperature 375 °C
Mold Temperature 170 - 200 °C
Dry Time 3.00 - 5.00 hour
@Temperature 120 - 150 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Gate>1 mm or 0.5 x part thickness
Runner>3.5mm
 >3mm Die/nozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450GL30 30% Glass Fiber Reinforced
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
VICTREX™ PEEK 150GL30 30% Glass Fiber Reinforced
VICTREX™ PEEK 150G / 151G Polyetheretherketone, Unreinforced
Overview of materials for Polyetheretherketone, Unreinforced

PVICT2 / 71826

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.