MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® R plus 573/70 A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Electrically conductive two component silicone rubber grades for extrusion of profiles and cable components in hot air.

Properties: The materials are black due to their conductivity.

Special features:

  • good mechanical and electrical properties
  • high conductivity
  • low volume resistivity
  • good heat resistance
  • good rheological properties
  • combustion products of low toxicity and corrosivity and low smoke density
  • none cross-linking agent crack products
  • flame retardant
Application: electrically conductive profiles, EMI-gaskets, ignition cables (core), band electrodes

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³DIN EN ISO 1183-1 A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272DIN 53505
Tensile Strength at Break 6.30 MPa914 psiDIN 53504 S1
Elongation at Break 250 %250 %DIN 53504 S1
Tear Strength 16.0 kN/m91.3 pliASTM D624 B
Compression Set 33 %
@Temperature 175 °C,
Time 79200 sec
33 %
@Temperature 347 °F,
Time 22.0 hour
post cured 4h/200°C; DIN ISO 815-B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.6 ohm-cm1.6 ohm-cmDIN IEC 93
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® R plus 573/50 A/B Silicone Rubber
Abatron L060421-1 Heat-Resistant Non-Flammable Silicone Rubber
Rogers Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate
Overview of materials for Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Silicone Rubber

PWACK9257 / 204786

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.