MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chengdu Letain T — 5130P Coating
Categories: Other Engineering Material

Material Notes: LTPT-5000 serials are crystal whisker and nano-filler reinforced coating materials with high performance based on PPS and PAI resin. The coating has great adhesive power to carbon steel, aluminous and low carbon stainless steel. It construction technology is quite simple. For its resistance to elevated temperature, acid and alkali, and friction, the materials are extensively applied in corrosion protection coating, non-stick coating, high temperature insulation coating, electrostatic prevention coating and heat conduction coating.

Usage: 1)suitable for suspension spray painting, hot spraying and electrostatic spraying.

Usage: 2) can be used in company with TPFE, PEEK, PES, PAI.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Grain Size <= 74 µm<= 74 µm
 
Descriptive Properties
ColorPale yellow powder
Film forming rigidity10
Film forming thickness10-200
Solidification temperature360-420

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT053 / 255906

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.