MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Trigonox F-CL50 tert-Butyl peroxyacetate, 50% solution in isoparrafin
Categories: Other Engineering Material

Material Notes: Trigonox F-CL50 is an efficient initiator (50% active ingredient in isoparrafin) for the production of Low Density Polyethylene (LDPE). It is used for both tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range.

CAS number: 107-71-1

EINECS/ELINCS No: 203-514-5

Applications: Polymerization of ethylene: Trigonox F-CL50 is an efficient initiator for the ethylene polymerization under high pressure in both autoclave and tubular processes. To obtain a wide spectrum of polymerization temperatures, combinations with other peroxides are applied in practice.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.820 g/cc
@Temperature 20.0 °C
0.0296 lb/in³
@Temperature 68.0 °F
Half-life  0.100
@Temperature 139 °C
0.100
@Temperature 282 °F
[hr]
 1.00
@Temperature 119 °C
1.00
@Temperature 246 °F
[hr]
 10.0
@Temperature 100 °C
10.0
@Temperature 212 °F
[hr]
Viscosity 1.5 cP
@Temperature 10.0 °C
1.5 cP
@Temperature 50.0 °F
Molecular Weight 132.2 g/mol132.2 g/mol
Storage Temperature -15.0 - 10.0 °C5.00 - 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 70.0 °C158 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay49.0-51.0 %
Color= 20 Pt-Co / APHA
Content= 0.15 %Hydroperoxides as TBHP
 5.93-6.17 %Active oxygen
Content (%)12.11Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1195 / 286718

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.