MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Johnson Matthey Active-braze™ No. 15 Brazing Paste Grade B420P 75 & B420P80
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Active-braze™ No.15 Brazing Paste is a specialized brazing paste for the active brazing of non-metallic materials. Employing an active brazing technique removes the need for prior metallization of the non-metallic material such as the ‘moly-manganese’ metallization commonly applied to alumina ceramics.

Active-braze™ No.15 brazing paste is formulated around a silver-copper-indium filler metal with an addition of titanium as the active element. The paste binder system used in the product is a water soluble polymer type.

Active type brazing filler metals do not flow by capillary attraction or spread significantly like most brazing filler metals and need to be placed within the joint. Active-braze™ No.15 has a brazing temperature range of 720 to 860°C.

Active-braze™No.15 is used for the brazing of ceramics like alumina and zirconia, diamond, natural, single crystal, or CVD (chemical vapor deposition) types, as well as graphite, sapphire, silicon carbide, PCD (polycrystalline diamond) and PCBN (polycrystalline cubic boron nitride) to themselves or to metallic substrates like low expansion nickel alloys, copper and tungsten carbide.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 620 - 720 °C1150 - 1330 °F
Solidus 620 °C1150 °F
Liquidus 720 °C1330 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 24 %24 %
Indium, In 14 %14 %
Silver, Ag 60 %60 %
Titanium, Ti 2.0 %2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Boron Nitride, Cubic BN, (Borazone)
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating
Boron Nitride, 60% SiO2 - 40% BN
Cobalt, Co
Johnson Matthey Active-braze™ No. 10 Brazing Paste Grade B420P 75

NJMMJ9899 / 186300

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.