MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.

Data provided by the manufacturer, Wellman Inc.

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
Water Absorption 1.2 %1.2 %Approximate 24 hr.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 210 MPa30500 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Flexural Yield Strength 310 MPa45000 psiISO 178
Flexural Modulus 12.5 GPa1810 ksiISO 178
Izod Impact, Notched 1.30 J/cm2.44 ft-lb/inISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75
Flammability, UL94 HB
@Thickness 0.790 mm
HB
@Thickness 0.0311 in
From Wellman QC Laboratory Testing; UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 282 - 310 °C540 - 590 °F
Middle Barrel Temperature 277 - 304 °C530 - 580 °F
Front Barrel Temperature 271 - 299 °C520 - 570 °F
Nozzle Temperature 271 - 304 °C520 - 580 °F
Melt Temperature 271 - 304 °C520 - 580 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 79.4 °C175 °FOpened bags and gaylord boxes
Dry Time 2 - 4 hour2 - 4 hourOpened bags and gaylord boxes
Moisture Content 0.050 - 0.20 %0.050 - 0.20 %During molding to prevent hydrolytic degradation
 <= 0.20 %<= 0.20 %In shipping bags, ready to mold
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Back Pressure 0.345 MPa50.0 psi
Screw Speed 30 - 120 rpm30 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wellman Wellamid® GF13-66 XE-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
RTP Company RTP 699 X 94678 SSC-63386 Acrylonitrile Butadiene Styrene (ABS), Phosphorescent Green
RTP Company RTP 199 X 98590 SSC-63791 Polypropylene (PP), Phosphorescent Green
Permabond HM128 Anaerobic Threadlocker
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding

PWEL18 / 72298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.