MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toray PMC CFRT® XRP 116 Reinforced Polypropylene Laminate
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 60% Glass Fiber Filler

Material Notes: Toray PMC CFRT® (XRP) is a reinforced thermoplastic composite laminate that brings innovative technology to orthotic and glass fiber reinforcement with polypropylene (PP) applications. It satisfies both the workshop need for ease of fabrication and the patient need for comfort and performance. Parts and devices made from thermoplastic sheets, of polypropylene, are reinforced in strategic locations by thermobonding the XRP panel to the polypropylene part during vacuum forming or drape molding. The result is a part with increased strength and stiffness, without having to raise the basic sheet thickness. We offer XRP in four different grades.

Features:

  • Glass fibers for maximum reinforcement
  • Increased strength and stiffness of local areas
  • Polypropylene matrix, to heat weld to polypropylene and copolymer materials
  • Thin and lightweight
  • Allows reduction of part thickness
  • Easily molded to deep contours
  • Can be adjusted with local heat
Product Type And Composition: Glass fiber content: 55%; Polypropylene: 45% (Nominal volume percentages)

Typical Applications:

  • Braces
  • Foot inserts
  • Reinforcements
  • Sockets

Information provided by Toray Performance Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3320 microns
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 7.10 GPa
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °CForming
 
Descriptive Properties
ColorsGray
Rigidity2330 N-cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY8085 / 265483

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.