MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes:

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ISO 1183
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.2 %1.2 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00040 cm/cm
@Thickness 2.00 mm
0.00040 in/in
@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psiConditioned; ISO 527-2
 240 MPa34800 psiDry; ISO 527-2
Elongation at Break 2.5 %2.5 %Dry; ISO 527-2
 2.8 %2.8 %Conditioned; ISO 527-2
Tensile Modulus 15.2 GPa2200 ksiConditioned; ISO 527-2
 16.8 GPa2440 ksiDry; ISO 527-2
Flexural Strength 270 MPa39200 psiConditioned; ISO 178
 350 MPa50800 psiDry; ISO 178
Flexural Modulus 11.2 GPa1620 ksiConditioned; ISO 178
 16.0 GPa2320 ksiDry; ISO 178
Poissons Ratio 0.400.40Dry; ISO 527-2
Izod Impact, Notched (ISO)  16.0 kJ/m²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 180
 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 180
 18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 180
 21.0 kJ/m²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 180
Charpy Impact Unnotched  9.10 J/cm²
@Temperature -30.0 °C
43.3 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 2.10 J/cm²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm
@Thickness 0.750 mm
1.00e+12 ohm-cm
@Thickness 0.0295 in
IEC 60093
Dielectric Strength 20.0 kV/mm
@Thickness 1.00 mm
508 kV/in
@Thickness 0.0394 in
IEC 60243
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
120 - 180 sec
@Thickness 0.118 in
PLC 5; ASTM D495
Comparative Tracking Index 400 - 599 V
@Thickness 3.00 mm
400 - 599 V
@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness 0.750 mm
7.0 - 15 sec
@Thickness 0.0295 in
PLC 4; UL 746
 7.0 - 15 sec
@Thickness 3.00 mm
7.0 - 15 sec
@Thickness 0.118 in
PLC 4; UL 746
 15 - 30 sec
@Thickness 1.50 mm
15 - 30 sec
@Thickness 0.0591 in
PLC 3; UL 746
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
PLC 0; UL 746
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
PLC 0; UL 746
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
PLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minPLC 1; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 12.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.67 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 260 °C500 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75-2/A
UL RTI, Electrical  140 °C
@Thickness 0.750 mm
284 °F
@Thickness 0.0295 in
UL 746
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL 746
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  140 °C
@Thickness 0.750 mm
284 °F
@Thickness 0.0295 in
UL 746
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL 746
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Flame Spread 0.000 mm/min
@Thickness 2.00 mm
0.000 in/min
@Thickness 0.0787 in
ISO 3795
Glow Wire Ignition Temperature  700 °C
@Thickness 0.750 mm
1290 °F
@Thickness 0.0295 in
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-13
 750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  675 °C
@Thickness 0.750 mm
1250 °F
@Thickness 0.0295 in
IEC 60695-2-12
 675 °C
@Thickness 1.50 mm
1250 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection Molding
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection Molding
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection Molding
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection Molding
Melt Temperature 285 - 305 °C545 - 581 °FInjection Molding
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection Molding
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Injection Molding
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes
FDA YesYes21 CFR 177.1500
 
Descriptive Properties
Agency RatingsASTM D 4066 PA012G50
 ASTM D 6779 PA012G50
 EU 10/2011
 EU 2023/2006
 SAE J1639 PA1116
Automotive SpecificationsGM GMW3038P-PA66-GF50H
 GM GMW3038P-PA66-GF50J
FeaturesGood Flow
 Good Mold Release
 Heat Stabilized
 High Rigidity
 High Strength
 Lubricated
Suggested Max Regrind (%)25
UsesAutomotive Under the Hood
 Gears
 Housings
 Power/Other Tools

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® R550H BK02 Nylon 66, 50% Glass Filled
Asahi Kasei Thermylene® P6-50FG-0100 PP-GF50
Techmer ES HiFill® PP GB50 50% Glass Beads Filled
Envalior Arnite® TV4 290 PBT-GF50
EMS-Grivory Grilon® BK-50 PA6-GB50

PZASCE9839 / 220940

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.