MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: OREVAC® 18211 is maleic anhydride grafted EVA copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 18211 provides outstanding adhesion to PS, PE, PA, EVOH. It is typically used in coextrusion of multilayer structures used in flexible or rigid packaging.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183
Melt Index of Compound 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 27ISO 608
Tensile Strength at Break 29.3 MPa
Tensile Strength, Yield 5.10 MPaASTM D638
Elongation at Break 550 %ASTM D638
Dart Drop Test 260 gASTM D1709
 
Thermal PropertiesOriginal ValueComments
Melting Point 75.0 °CDSC
Vicat Softening Point 51.0 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 5.2 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Orevac® 18216 Maleic Anhydride modified EVA
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Arkema OREVAC® 9304 EVA Terpolymer
Arkema Orevac® 9304 Film EVA-MAH Terpolymer
Arkema Orevac® 9307 Y Film EVA-MAH Terpolymer

PARKG112 / 80104

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.