OREVAC® 18211 is maleic anhydride grafted EVA copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 18211 provides outstanding adhesion to PS, PE, PA, EVOH. It is typically used in coextrusion of multilayer structures used in flexible or rigid packaging.Information provided by Arkema Group |