MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Clariant PA6/66-GF20 FR LS Using Exolit® Flame Retardant Nylon 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 20% Glass Fiber Reinforced

Material Notes: PA6/66-GF20 FR LS using Exolit® is a newly developed flame retardant material that is compliant with EN 45545-2, NFPA 130 (ASTM E162, ASTM E662) and SMP 800-C. This material was designed specifically for 3D printing to achieve ideal mechanical properties with excellent flame retardancy, low smoke and low toxicity. The material is ideal for the production of end use parts using printers with enclosed or heated chambers.

Information provided by Clariant.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.293 g/ccISO 1183
pH 4.3 - 4.51% in water
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 46.0 MPa
@Temperature 23.0 °C
XY Direction Flat; ISO 527
 52.0 MPa
@Temperature -40.0 °C
XY Direction Flat; ISO 527
 53.0 MPa
@Temperature -40.0 °C
XZ Direction on Edge; ISO 527
Elongation at Break 1.7 %
@Temperature -40.0 °C
XZ Direction on Edge; ISO 527
 2.1 %
@Temperature -40.0 °C
XY Direction Flat; ISO 527
 2.5 %
@Temperature 23.0 °C
XY Direction Flat; ISO 527
Modulus of Elasticity 4.00 GPa
@Temperature 23.0 °C
XY Direction Flat; ISO 527
 4.06 GPa
@Temperature -40.0 °C
XY Direction Flat; ISO 527
 4.88 GPa
@Temperature -40.0 °C
XZ Direction on Edge; ISO 527
Flexural Strength 147 MPaInjection Molded; ISO 178
Flexural Modulus 5590 MPaInjection Molded; ISO 178
Charpy Impact, Notched 13.1 kJ/m²XY Direction Flat; ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 195 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 168 °CXY Direction Flat; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 114 °CXY Direction Flat; ISO 75
Flammability, UL94 V-2
@Thickness 0.400 mm
XY Direction Flat
 V-2
@Thickness 0.800 mm
XY Direction Flat
 V-1
@Thickness 1.60 mm
XY Direction Flat
 V-0
@Thickness 3.20 mm
XY Direction Flat
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 230 - 250 °C
 
Descriptive Properties
Bed temperature (°C)80
Printing speed (mm/s)20 - 50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCLAR00037 / 291049

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.