MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Applications
  • Extrusion
  • Injection
  • Compounding
  • Industry Parts
  • Parts for Automobile/Mobile phone
  • Acetal Compound

Information provided by API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282ASTM D2240
Tensile Strength 44.1 MPa6400 psiASTM D412
Tensile Stress at Strain 5.20 MPa
@Strain 100 %
754 psi
@Strain 100 %
ASTM D412
Elongation at Break 563 %563 %ASTM D412
Tear Strength 100 kN/m571 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 185 - 195 °C365 - 383 °FInjection Molding
Zone 1 155 - 170 °C311 - 338 °FExtrusion Molding
 160 - 175 °C320 - 347 °FInjection Molding
Zone 2 170 - 180 °C338 - 356 °FExtrusion Molding
 175 - 185 °C347 - 365 °FInjection Molding
Zone 3 180 - 190 °C356 - 374 °FInjection Molding
 180 - 190 °C356 - 374 °FExtrusion Molding
Zone 4 185 - 195 °C365 - 383 °FExtrusion Molding
Die Temperature 185 - 195 °C365 - 383 °FExtrusion Molding
Head Temperature 190 - 200 °C374 - 392 °FExtrusion Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
Abatron 223 A/B Filled Potting Compound
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Asahi Kasei TENAC™-C HC350 Copolymer Acetal (POM)
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer

PKOKZ989 / 122691

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.