MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Powersil® GEL FC A/B Silicone Gel
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® GEL FC A/B is a pourable, addition curing, two-component silicone rubber that vulcanizes at room temperature to a soft silicone gel. POWERSIL® GEL FC A/B shows a very fast curing behavior.

Special features:

  • fast curing
  • two-part, 1 : 1 mixing ratio
  • very low viscosity
  • very low hardness (silicone gel)
  • transparent vulcanizate
  • pronounced tackiness
  • excellent mechanical damping properties
Application:
  • sealing of MV and HV cable joints
  • LV easy-to-use cable joints
  • castings and sealants of electrical equipment

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ISO 1183-1 A
Viscosity 1000 cP1000 cPComponent A; ISO 3219
 1000 cP1000 cPComponent B; ISO 3219
 1000 cP
@Shear Rate 0.890 1/s
1000 cP
@Shear Rate 0.890 1/s
Mixed; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Penetration 180
@Load 0.150 kg
180
@Load 0.331 lb
1/10 mm, hollow cone; ISO 2137
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 50 Hz
2.5
@Frequency 50 Hz
IEC 60250
Dielectric Strength 23.0 kV/mm584 kV/inIEC 60243
Dissipation Factor 0.00020
@Frequency 50 Hz
0.00020
@Frequency 50 Hz
IEC 60250
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Component A. "Transparent" but manufacturer does not quantify.
 90 %90 %Component B. "Transparent" but manufacturer does not quantify.
 90 %90 %cured. "Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time  3.00 min
@Treatment Temp. 100 °C
0.0500 hour
@Treatment Temp. 212 °F
 6.00 min
@Treatment Temp. 50.0 °C
0.100 hour
@Treatment Temp. 122 °F
 30.0 min
@Treatment Temp. 150 °C
0.500 hour
@Treatment Temp. 302 °F
circulating air oven
 35.0 min
@Treatment Temp. 23.0 °C
0.583 hour
@Treatment Temp. 73.4 °F
Pot Life 20.0 min20.0 min
 
Descriptive Properties
ColortransparentComponent A
 transparentComponent B
 transparentcured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SMAC SMACWRAP® ST Damping Material, 1 mm
Wacker Elastosil® R 401/10 Silicone Rubber
SMAC SMACMOUNT® 2528S 02 Damping Material
SMAC SMACFOAM® 1250S-01 Damping Material
SMAC BARRIER® Damping Material

PWACK9393 / 204922

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.