MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
E-Polymers SEPAZ® C240GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding productivity. SEPAZ LCP has a unique attribute in that the thinner the product becomes, the greater the mechanical strength. SEPAZ LCP finds uses in connectors, sensors and other electronic components and CD pick-up parts, and in copying machine and fax components in office and audio-visual equipment.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 g/ccASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 130.5 MPaASTM D638
Elongation at Break 1.5 %ASTM D638
Flexural Strength 181.49 MPaASTM D790
Flexural Modulus 12753 MPaASTM D790
Izod Impact, Notched 4.00 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 352 °CASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 300 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 370 °C
Mold Temperature 40.0 - 150 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zenite® 9140HT NC010 LCP
Celanese VECTRA T.rex541 LCP, 40% Specialty
Celanese Zenite® 7140X BK010 LCP
Avient Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding
Celanese VECTRA® L140 40% Glass Reinforced Liquid Crystal Polymer (LCP)

PEPOLZ069 / 103566

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.