MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® R 861/60 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: These translucent compounds are highly flexible and are noted for their low compression set and improved medium resistance.

Application: This compound can be used in the manufacture of molded parts, but also particularly for producing profiles, e. g. for windows and facades. Provided appropriate processing, articles produced from ELASTOSIL® R 861/60 can be used for food contact applications in accordance with the Recommendation "XV. Silicones" of the BfR and FDA 21 CFR § 177.2600 under observance of any given limitations on extractable and volatile substances. Furthermore, the product contains low levels of residual toluene which has to be completely removed from the final food contact article.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183-1 A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5656curing agent E; DIN 53505
 6060curing agent C1
 6060oil storage
 6161cooling agent immersion
 41
@Treatment Temp. 150 °C,
Time 259000 sec
41
@Treatment Temp. 302 °F,
Time 72.0 hour
IRM 903 oil resistance, C6 crosslinker
 54
@Treatment Temp. 150 °C,
Time 259000 sec
54
@Treatment Temp. 302 °F,
Time 72.0 hour
IRM 901 oil resistance, C6 crosslinker
 58
@Treatment Temp. 125 °C,
Time 3.629e+6 sec
58
@Treatment Temp. 257 °F,
Time 1008 hour
after immersion, crosslinker C1
Tensile Strength at Break 8.30 MPa1200 psicuring agent E; DIN 53504 S1
 8.50 MPa1230 psicuring agent C1; DIN 53504 S1
 9.40 MPa1360 psicooling agent immersion
 9.90 MPa1440 psioil storage
 7.90 MPa
@Treatment Temp. 125 °C,
Time 3.629e+6 sec
1150 psi
@Treatment Temp. 257 °F,
Time 1008 hour
after immersion, crosslinker C1
 8.00 MPa
@Treatment Temp. 150 °C,
Time 259000 sec
1160 psi
@Treatment Temp. 302 °F,
Time 72.0 hour
IRM 903 oil resistance, C6 crosslinker
 9.10 MPa
@Treatment Temp. 150 °C,
Time 259000 sec
1320 psi
@Treatment Temp. 302 °F,
Time 72.0 hour
IRM 901 oil resistance, C6 crosslinker
Elongation at Break 370 %370 %curing agent E; DIN 53504 S1
 405 %405 %cooling agent immersion
 420 %420 %curing agent C1; DIN 53504 S1
 480 %480 %oil storage
 292 %
@Treatment Temp. 150 °C,
Time 259000 sec
292 %
@Treatment Temp. 302 °F,
Time 72.0 hour
IRM 903 oil resistance, C6 crosslinker
 354 %
@Treatment Temp. 125 °C,
Time 3.629e+6 sec
354 %
@Treatment Temp. 257 °F,
Time 1008 hour
after immersion, crosslinker C1
 372 %
@Treatment Temp. 150 °C,
Time 259000 sec
372 %
@Treatment Temp. 302 °F,
Time 72.0 hour
IRM 901 oil resistance, C6 crosslinker
Rebound 52 %52 %curing agent E; DIN 53512
 53 %53 %curing agent C1; DIN 53512
Tear Strength 16.0 kN/m91.3 plicuring agent C1; ASTM D624 B
 16.0 kN/m91.3 plicuring agent E; ASTM D624 B
Compression Set  10 %
@Temperature 175 °C,
Time 79200 sec
10 %
@Temperature 347 °F,
Time 22.0 hour
curing agent C1; DIN ISO 815-B
 15 %
@Temperature 175 °C,
Time 252000 sec
15 %
@Temperature 347 °F,
Time 70.0 hour
curing agent C1; DIN ISO 815-B
 16 %
@Temperature 175 °C,
Time 79200 sec
16 %
@Temperature 347 °F,
Time 22.0 hour
curing agent E; DIN ISO 815-B
 30 %
@Temperature 175 °C,
Time 252000 sec
30 %
@Temperature 347 °F,
Time 70.0 hour
curing agent E; DIN ISO 815-B
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Appearancetranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3071/60 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3005/60 A/B Liquid Silicone Rubber
Wacker ELASTOSIL® R 427/70 High Strength Silicone Base
Wacker Elastosil® R 420/70 Silicone Rubber

PWACK9246 / 204775

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.