MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Random Copolymer for Containers, Totes and Bins, and Closures

Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for injection molding including thin wall applications. The use of an advanced clarifier with low yellowness index and haze – makes it an excellent choice for ‘see-through’ housewares and rigid packaging. Use of this clarifier allows processers to run at lower temperatures - resulting in the potential for cycle time reductions and energy savings

Formolene® 3355E meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.

Specimens were injection molded according to the conditions specified in ASTM D4101

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 55 g/10 min
@Temperature 230 °C
I2; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4200 psi2" (50mm) per min; ASTM D638
Elongation at Yield 15 %2" (50mm) per min; ASTM D638
Flexural Modulus, 1% Secant 150000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Temperature 23.0 °C
ASTM D256A
Gardner Impact 20.0 JASTM D5420
 180 in-lbASTM D2794
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 178 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 10 %
@Thickness 1.00 mm
Plaque; FPC method
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 3335E Random Copolymer Polypropylene
Braskem INSPIRE™ 222 Performance Polypropylene Polymer
Flint Hills P5M4K-046 Random Copolymer Polypropylene
Formosa Plastics Formolene® 3355O Random Copolymer Polypropylene
Formosa Plastics Formolene® 3435E Random Copolymer Polypropylene

PFPCPQ037 / 150269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.