MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik 316-5R60 Billet
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Austenitic stainless steel, AISI 316/316H

Sandvik 5R60 is an austenitic chromium-nickel steel with minimum 2.5% molybdenum and a controlled carbon content in order to obtain improved strength at high temperatures.

Information provided by Sandvik

ASTM 316; UNS S31600; EN 1.4436

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 170
Tensile Strength, Ultimate 515 - 690 MPa
 >= 360 MPa
@Temperature 500 °C
 >= 380 MPa
@Temperature 300 °C
 >= 380 MPa
@Temperature 400 °C
 >= 400 MPa
@Temperature 200 °C
 >= 450 MPa
@Temperature 100 °C
Tensile Strength, Yield >= 205 MPa
@Strain 0.2 %
 >= 240 MPa
@Strain 1 %
 >= 92.0 MPa
@Strain 0.2 %,
Temperature 500 °C
 >= 98.0 MPa
@Strain 0.2 %,
Temperature 400 °C
 >= 110 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 120 MPa
@Strain 1 %,
Temperature 500 °C
 >= 125 MPa
@Strain 1 %,
Temperature 400 °C
 >= 127 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 130 MPa
@Strain 1 %,
Temperature 300 °C
 >= 155 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 155 MPa
@Strain 1 %,
Temperature 200 °C
 >= 190 MPa
@Strain 1 %,
Temperature 100 °C
Elongation at Break >= 40 %
Reduction of Area >= 50 %
Charpy Impact 100 J
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 %
Chromium, Cr 17 %
Iron, Fe 66.2 %As Balance
Manganese, Mn 1.7 %
Molybdenum, Mo 2.6 %
Nickel, Ni 12 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.40 %
Sulfur, S <= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
316 Stainless Steel, annealed plate
347 Stainless Steel, annealed, sheet
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
Kinetics MIM 316 Stainless Steel (Standard Grade)
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600

NSANDV153 / 19047

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.