MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mitsubishi Chemical Advanced Materials TIVAR® 1000 (Natural & Color except Black) UHMW-PE  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: Ultrahigh-molecular-weight Polyethylene
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc
@Temperature 22.8 °C
0.930 g/cc
@Temperature 73.0 °F
ASTM D792
Water Absorption at Saturation 0.010 %0.010 %ASTM D570 2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 66
@Temperature 22.8 °C
66
@Temperature 73.0 °F
ASTM D2240
Tensile Strength 40.0 MPa
@Temperature 22.8 °C
5800 psi
@Temperature 73.0 °F
ASTM D638
Tensile Modulus 0.552 GPa
@Temperature 22.8 °C
80.0 ksi
@Temperature 73.0 °F
ASTM D638
Flexural Strength 24.1 MPa
@Temperature 22.8 °C
3500 psi
@Temperature 73.0 °F
ASTM D790
Compressive Strength 20.7 MPa
@Temperature 22.8 °C
3000 psi
@Temperature 73.0 °F
ASTM D695
Compressive Modulus 0.552 GPa
@Temperature 22.8 °C
80.0 ksi
@Temperature 73.0 °F
ASTM D695
Shear Strength 33.1 MPa
@Temperature 22.8 °C
4800 psi
@Temperature 73.0 °F
ASTM D732
Coefficient of Friction, Dynamic 0.120.12QTM 55007
Sand Slurry 10101018 Steel = 100; ASTM D4020
Limiting Pressure Velocity 0.105 MPa-m/sec3000 psi-ft/min(with 4:1 safety factor applied); QTM 55007
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 45.3 kV/mm1150 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.409 W/m-K2.84 BTU-in/hr-ft²-°FASTM E 1530-11
Melting Point 135 °C275 °FASTM D3418

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 EC UHMW-PE Electrically Conductive
RTP Company RTP 2285 A Polyetherketone (PEK), Carbon Fiber
VICTREX HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight

P1SMP00A / 171660

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.