MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Geniosil® XL 926 Silane
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C13H29NO3Si

CAS No.: 26495-91-0

Properties: GENIOSIL® XL 926 binds via its aminomethyl group to electrophilic groups in resins and polymers. Aside from groups such as epoxides and esters, it is particularly the isocyanate groups present in polyurethanes that are important here. GENIOSIL® XL 926 is characterized by its high reactivity toward moisture, a direct consequence of the nitrogen atom's proximity to the silicon atom within the molecule (alpha-effect).The basicity of the secondary amino group renders GENIOSIL® XL 926 "autocatalytic" while the trialkoxysilyl moiety results in very high crosslinking density. GENIOSIL® XL 926 also offers advantages in all applications requiring high reactivity combined with the release of ethanol rather than methanol. By binding GENIOSIL® XL 926 to polymers such as polyurethanes, the manifold advantages of silane crosslinking can be transferred to other systems.

Special features: GENIOSIL® XL 926 is an (aminomethyl)alkylsilane. It´s a clear, colorless to light yellowish liquid with a characteristically aromatic odor. The silane hydrolyzes in the presence of moisture (ethanol is released) to form silanols, which can then react with themselves to produce siloxanes. The close proximity of the nitrogen atom to the silicon atom results in a greatly accelerated hydrolysis reaction compared to (aminopropyl) silanes (alpha-effect).

Application: GENIOSIL® XL 926 is used in the production of silylmodified polymers which serve as binders in adhesives and sealants. Of particular importance is the reaction with materials containing isocyanate groups (PU prepolymers). GENIOSIL® XL 926 is also used as a crosslinker, water scavenger and adhesion promoter in silane crosslinking formulations, such as adhesives, sealants and coatings.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9514 g/ccDIN 51757
Kinematic Viscosity 3.27 cSt
Molecular Weight 275.5 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 236 °C
@Pressure 0.1013 MPa
Flash Point 119 °CEN 22719
Ignition Temperature 225 °Cliquids; DIN 51794
 
Descriptive Properties
Purity>95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9339 / 204868

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.