MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® TS92AP7 NAT 055 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Estane® TS92AP7 NAT 055 is an aromatic polycarbonate-based thermoplastic polyurethane.

Features: Extrusion

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ISO 868
Tensile Strength 60.0 MPa8700 psiISO 527-2/5A/500
Elongation at Break 375 %375 %ISO 527-2/5A/500
50% Modulus 14.0 MPa
@Strain 50 %
14.0 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 18.0 MPa
@Strain 100 %
2610 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 44.0 MPa
@Strain 300 %
6380 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 103 kN/m588 plinicked; ISO 34-1B
Abrasion 3939[mm3]; ISO 4649-B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 82.0 °C180 °FA50; ISO 306
 
Processing PropertiesMetricEnglishComments
Zone 1 200 °C392 °F
Zone 2 205 °C401 °F
Zone 3 210 °C410 °F
Zone 4 210 °C410 °F
Adapter Temperature 210 °C410 °F(5)
Die Temperature 200 °C392 °FTIP (7)
 205 °C401 °F(6)
Drying Temperature 100 °C
@Time 10800 - 14400 sec
212 °F
@Time 3.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR5026 / 238896

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.