System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LNP™ THERMOCOMP™ Compound DX07408 Polycarbonate (PC)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
LNP THERMOCOMP DX07408 compound is based on Polycarbonate (PC) resin containing 40% glass fiber. Added features of this grade include: Flame Retardant.
Features: High Stiffness,Flame Retardant,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.50
g/cc
ASTM D792
Density
1.50
g/cc
ASTM D792
Moisture Absorption
0.0200 %
Injection Molding
0.0900 %
23°C/50% RH/24 hrs; ASTM D570
0.150 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0010
-
0.0040
cm/cm
24hrs; ASTM D955
Linear Mold Shrinkage, Transverse
0.0060
-
0.0090
cm/cm
24hrs; ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
120
MPa
5 mm/min; ASTM D638
126
MPa
5 mm/min; ISO 527
Tensile Strength, Yield
120
MPa
5 mm/min; ASTM D638
126
MPa
5 mm/min; ISO 527
Elongation at Break
2.0 %
5 mm/min; ASTM D638
2.2 %
5 mm/min; ISO 527
Elongation at Yield
2.0 %
5 mm/min; ASTM D638
2.2 %
5 mm/min; ISO 527
Tensile Modulus
10040
MPa
1 mm/min; ISO 527
10360
MPa
5 mm/min; ASTM D638
Flexural Strength
172
MPa
ISO 178
179
MPa
brk, 1.3 mm/min, 50 mm span; ASTM D790
179
MPa
yld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
9100
MPa
2 mm/min; ISO 178
9570
MPa
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
100
J
ASTM D256
Izod Impact, Unnotched
581
J/m
ASTM D4812
Izod Impact, Notched (ISO)
9.00
kJ/m²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
39.0
kJ/m²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
17.0
J
ASTM D3763
Impact Test
3.00
J
Multiaxial Impact; ISO 6603
Electrical Properties
Original Value
Comments
Arc Resistance
0.00
-
60
sec
ASTM D495
Comparative Tracking Index
100
-
175
V
UL 746A
Hot Wire Ignition, HWI
>=
120
sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI
0.00
-
15
arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR
80.0
-
150
mm/min
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
21.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow
55.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
139
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
139
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
134
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
135
°C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical
130
°C
UL 746B
UL RTI, Mechanical with Impact
130
°C
UL 746B
UL RTI, Mechanical without Impact
130
°C
UL 746B
Flammability, UL94
V-1
@Thickness >=1.10 mm
UL 94
V-0
@Thickness >=1.50 mm
UL 94
Processing Properties
Original Value
Comments
Zone 2
310
-
320
°C
Zone 3
320
-
330
°C
Melt Temperature
305
-
325
°C
Injection Molding
Mold Temperature
80.0
-
110
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
Screw Speed
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH81554 / 289501
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.