MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tabriz 6070 UA HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HD6070UA is high density polyethylene copolymer containing butene-1(C4) as comonomer with medium content of light stabilizer additives. It is suitable for general purpose injection molding items. HD6070UA has good impact strength, easy processing, high warpage resistance, high rigidity, UV stabilized. This grade has food contact approval. Applications: crates, boxes, seats.

Information provided by Tabriz Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D1505
Brightness 60.0 %Whiteness Index; ASTM E313
Melt Flow 7.0 g/10 min
@Load 2.16 kg
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPaASTM D638
Elongation at Break 900 %ASTM D638
Charpy Impact, Notched 5.00 kJ/m²ASTM D6110
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 120 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Yellow Index -1.00 %ASTM E313
 
Descriptive Properties
Contamination (No.)5BP137

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SIDPEC EGYPTENE® HD 6070 UA HDPE Injection Molding
INEOS Styrolution Novodur® HD M203FC Acrylonitrile Butadiene Styrene (ABS)
Celanese Hostaform® MT24U01 POM, Medical Technology
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Tabriz FC522 Performance Expandable Polystyrene

PIPC036 / 48264

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.