MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Product Characteristics
  • High Gloss/High Impact
  • Consistent colorability
  • Easy processing
  • Food Contact Compliant

Typical Applications

  • Custom high Gloss Extruded Sheet
  • Refrigeration accessories
  • Small Appliances

Information provided by AmericasStyrenics LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 in/inASTM D955
Melt Flow 2.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102.5ASTM D785
Tensile Strength at Break 2800 psiASTM D638
Tensile Strength 3900 psiASTM D638
Elongation at Break 50 %ASTM D638
Tensile Modulus 265 ksiASTM D638
Flexural Strength 5200 psiASTM D790
Flexural Modulus 270 ksiASTM D790
Izod Impact, Notched 1.80 ft-lb/incompression molded; ASTM D256
 3.90 ft-lb/ininjection molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 192 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 173 °FASTM D648
Vicat Softening Point 214 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical HI121H ABS, High Stiffness
Entec Hypro™ F PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled
Entec Hypro™ F PPC-T20 Copolymer Polypropylene, 20% Talc Reinforced
Chi Mei Polylac® PA-757 ABS
Entec Hypro™ F PPC-GF15 Natural Impact Polypropylene, 15% Glass Reinforced

PAMERI931 / 131198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.