Potters Industries’ Oil Drilling Fine Grade glass beads are designed for oil drilling mud applications to reduce friction and torque within deviated holes. Potters solid glass spheres act as tiny ball bearings to reduce friction and reduce differential pressure. The glass beads are a transparent, solid soda Lime glass, free of pits and excess air bubbles. The glass beads are chemically inert and do not affect the chemical characteristics of the mud system.Information provided by Potters Industries |