MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Semicosil® 2M2M Silane
Categories: Fluid

Material Notes: Empirical formula: C4H12O2S

CAS No.: 1112-39-6

SEMICOSIL® 2M2M is Dimethoxydimethylsilane of high purity.

Special features:

  • high purity
  • low metal content
  • low chloride content
  • low methanol content
Application: SEMICOSIL® 2M2M was developed for the semiconductor industry, e.g. as precursor for low dielectric constant interlayer dielectrics.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³DIN 51757
Molecular Weight 120 g/mol120 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -30.0 °C<= -22.0 °F
Boiling Point 78.0 °C
@Pressure 0.1013 MPa
172 °F
@Pressure 14.69 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3711.371
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearancecolorless, clear liquid
Assayby Gas Chromatography

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9412 / 204941

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.