MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³±0.03 g/cm³; DIN 53479
Filler Content 15 %15 %Glass Fiber Reinforcement
Melt Index of Compound 18 g/10 min
@Load 1.60 kg,
Temperature 250 °C
18 g/10 min
@Load 3.53 lb,
Temperature 482 °F
cm³/10min; ISO 1133
Ash 15 %15 %ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa
@Temperature 23.0 °C
9430 psi
@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 4.0 %
@Temperature 23.0 °C
4.0 %
@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 4.60 GPa
@Temperature 23.0 °C
667 ksi
@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched 6.70 J/cm²
@Temperature 23.0 °C
31.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.950 J/cm²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 224 °C435 °FISO 3146
Maximum Service Temperature, Air 135 °C275 °FContinuous (GTP 50% Tensile); IEC 60216
 170 °C338 °FShort Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FUnannealed; ISO 75-2/B
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Internal Method
Glow Wire Ignition Temperature 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
1.6 mm wire; Ignition Temperature; IEC 60695-2-13
 
Descriptive Properties
AdditiveUV Stabilizer
FeaturesFlame Retardant
 Halogen Free
 Low (to None) Phosphorus Content
FormsPellets
Generic MaterialPBT
Generic NamePolybutylene Terephthalate (PBT)
Regional AvailabilityAfrica & Middle East
 Europe
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergadur™ PB40 G15 blue Polybutylene Terephthalate (PBT)
Avient Bergamid™ A70 UF natur V0 Polyamide 66 (Nylon 66)
Avient Bergamid™ A70 G25 H U-SO Polyamide 66 (Nylon 66)
Avient Bergadur™ PB400 G30 UF UV Polybutylene Terephthalate (PBT)
Avient Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT)

PH0POL0770 / 145339

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.