SCG PP P980J is a high crystalline impact copolymer polypropylene resin. It is designed for compounding and high speed injection molding process. This resin is recommended for products that require high stiffness/impact balance. Applications: Automotive exterior/interior parts. Home appliances parts. Complicated industrial parts. Compounding. Features: High flow ability. High stiffness and impact balance. Information provided by SCG. |