Metallocene polyethylene antiblock masterbatch. This erucamide slip and antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require: - Reduced COF
- Minimal antiblock effect on optics
- Excellent strength
Applications: Typical blown film applications include: - Use with MarFlex™ D139 and MarFlex™ D143
- Recommended usage is 1 to 2%
- May also be used with conventional LLDPE
Information provided by Phillips |