MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group QM 254 60 Shore A, Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 254 is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin resistance. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 254 is exceptionally good where high durometer and dimensional stability are required. This material also has excellent thermal stability.

Key Features:

  • High durometer
  • Low viscosity
  • Casting resin resistance
  • Fast demold time
  • Excellent dimensional stability
  • Excellent thermal stability
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, epoxy resin casting, and rigid or foam polyurethane
  • Molds for technical articles and prototypes
  • Molds for furniture and picture frame replication

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccQM 254B, Uncatalyzed
 1.26 g/cc1.26 g/ccQM 254A, Uncatalyzed
Viscosity 3500 cP3500 cPCatalyzed
 6000 cP6000 cPQM 254B, Uncatalyzed
 45000 cP45000 cPQM 254A, Uncatalyzed
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inCured 3 days at 25°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060Cured 3 days at 25°C
Tensile Strength 6.89 MPa1000 psiCured 3 days at 25°C
Elongation at Break 140 %140 %Cured 3 days at 25°C
Tear Strength 15.8 kN/m90.0 pliCured 3 days at 25°C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FCured 3 days at 25°C
Minimum Service Temperature, Air -55.0 °C-67.0 °FCured 3 days at 25°C
 
Processing PropertiesMetricEnglishComments
Cure Time 480 - 720 min8.00 - 12.0 hourDemold time, Catalyzed
 4320 min
@Temperature 25.0 °C
72.0 hour
@Temperature 77.0 °F
Pot Life 60.0 min60.0 minCatalyzed
 
Descriptive Properties
ColorBeigeQM 254A, Uncatalyzed
 BlackQM 254B, Uncatalyzed
 BlackCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QM 258 60 Shore A, Addition Cure Moldmaking Material
CHT Group QM 263 60 Shore A, Inhibition Resistant, Addition Cure Moldmaking Material
CHT Group QM 261 60 Shore A, Addition Cure Moldmaking Material
CHT Group QLE 1037 60 Shore A, Addition Cure Elastomer for Coating Applications
CHT Group QLE 1035PLE 38 Shore A, Addition Cure Elastomer for Coating Applications

PACC2052 / 199440

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.