MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kotec Carbotex KV-75FD Polycarbonate, Food Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Features: Food contact, High viscosity, Mold release, Transparent
Applications: Household appliance, Kitchenware, Food packaging/containers

Information provided by Kotec Corporation

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cmASTM D995
Melt Flow 4.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120
Tensile Strength at Break 63.0 MPaASTM D638
Elongation at Break 120 %ASTM D638
Flexural Strength 88.0 MPaASTM D790
Flexural Modulus 2260 MPaASTM D790
Izod Impact, Notched 880 J/m
@Temperature 23.0 °C
V-Notched 1/8"; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mmASTM D149
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 110 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 135 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.58ASTM D542
Haze <= 1.0 %
@Thickness 3.00 mm
ASTM D1003
Transmission, Visible 89 %
@Thickness 3.00 mm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1400 R-5100 Polyphenylsulfone (PPSU)
Polyram RamTough PZ741 Polycarbonate, UV Stabilized
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Lotte Advanced Materials Infino® PCA-NH1015V Flame Retardant
LG Chemical Lupoy 1200-08 Polycarbonate Resin

PKOTEC042 / 93272

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.