MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Radici RADIPOL® DC95 Nylon 610
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: N° CAS. 9011-52-3

Description: 6,10, Medium-high viscosity

Typical Applications: Base polymer for compounding and extrusion

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO1183
Viscosity  90000 cP
@Shear Rate 8000 1/s,
Temperature 300 °C
90000 cP
@Shear Rate 8000 1/s,
Temperature 572 °F
Apparent shear
 100000 cP
@Shear Rate 7000 1/s,
Temperature 275 °C
100000 cP
@Shear Rate 7000 1/s,
Temperature 527 °F
Apparent shear
 400000 cP
@Shear Rate 400 1/s,
Temperature 300 °C
400000 cP
@Shear Rate 400 1/s,
Temperature 572 °F
Apparent shear
 500000 cP
@Shear Rate 500 1/s,
Temperature 275 °C
500000 cP
@Shear Rate 500 1/s,
Temperature 527 °F
Apparent shear
 1.00e+6 cP
@Shear Rate 90.0 1/s,
Temperature 300 °C
1.00e+6 cP
@Shear Rate 90.0 1/s,
Temperature 572 °F
Apparent shear
 1.30e+6 cP
@Shear Rate 100 1/s,
Temperature 275 °C
1.30e+6 cP
@Shear Rate 100 1/s,
Temperature 527 °F
Apparent shear
Viscosity Measurement 3.853.85Relative, Solvent: sulphuric acid 95.7%; Polyamide concentration:0.01 g/ml
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 66.0 MPa9570 psi5mm/min; ISO 527-2/1A
Elongation at Break 40 %40 %50mm/min, Nominal; ISO 527-2/1A
Elongation at Yield 4.5 %4.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 2.20 GPa319 ksi1mm/min; ISO 527-2/1A
Flexural Strength 83.0 MPa12000 psi2mm/min; ISO 178/1A
Flexural Modulus 1.96 GPa284 ksi2mm/min; ISO 178/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179 eU
Charpy Impact, Notched 0.740 J/cm²
@Temperature 23.0 °C
3.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179 eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FScanning rate 10°C/min; ISO 11357-1-3
 
Optical PropertiesMetricEnglishComments
Yellow Index <= 8.0 %<= 8.0 %
 
Descriptive Properties
Chip Size2.0x2.5x3.0 mm
ColorNatural
Granulometry1.7 g/100 chips

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI014 / 313515

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.