MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Esstech X-846-0000 Methacroyloxyethyl Maleate, C10H12O6
Categories: Polymer; Adhesive

Material Notes: HEMA maleate is a carboxylic acid-containing methacrylate that can function as an alternative to PMDM. It has been used in anaerobic adhesive applications. Listed on the Toxic Substance Control Act List. CAS # 51978-15-5.

Information provided by ESSTECH, Inc.

Key Words: C10H12O6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.225 g/cc1.225 g/cc
Viscosity 300 cP
@Temperature 25.0 °C
300 cP
@Temperature 77.0 °F
Molecular Weight 228.2 g/mol228.2 g/mol
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4811.481
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Descriptive Properties
Acidity (NaOH per g)140-180 mg
Color (APHA)< 300
MeHQ Inhibitor (ppm)200-300
Purity (%)> 80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese 50000873 Di-n-Butyl Maleate (DBM)
TIMCAL ENSACO™ 150G Conductive Carbon Black
Esstech X-756-0000 1,3-Glycerol Dimethacrylate/Maleate Adduct, C15H18O8
Chosun Refractories AC-1 Acid-Proof and Heat-Resistant Brick
Celanese 50000433 Dioctyl Maleate (DOM)

PESST019 / 108290

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.