MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 342-13ACC Single Component Low Viscosity Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 342-13ACC single component, low viscosity epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature in 24 hours or at elevated temperatures. TRA-BOND 342-13ACC adhesive may be used to bond semi-porous materials such as ferrite, where a physical, rather than a chemical, bond is required.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccMixed
Viscosity 700 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Adhesive Bond Strength 3000 psiLap shear, alum to alum, @ 25°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.00e+14 ohm-cm
@Temperature 100 °C
Dielectric Constant 4.4
@Frequency 1000 Hz
Dissipation Factor 0.0010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.200 W/m-K
@Temperature 121 °C
Glass Transition Temp, Tg 99.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 95.0 °C
 2.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
 30.0 min
@Temperature 120 °C
Working Life 4.00 hour
@Temperature 25.0 °C
Shelf Life 12.0 Month
@Temperature -40.0 °C
 
Descriptive Properties
Thixotropic Index 1
Weight Loss % 0.85At 250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC114 / 71042

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.