MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, fire resistance, abrasion resistance; low-smoke emission; high purity

Applications:

  • Chemical processing – production, storage and transfer of corrosive fluids
  • Electronics – protective sheathing, plenum and wiring insulation
  • Semi-conductor industry
  • Food stuff and Healthcare industries
  • Transportation – fuel line and pipe, thermoformed body components

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.84 - 1.88 g/ccASTM D792
Density 1.88 g/cc
@Temperature 230 °C
Melt
Water Absorption 0.020 %Dry; Sim. to ISO 62
Viscosity 800000 - 1.30e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0070 cm/cmDry; ISO 294-4, 2577
 0.0070 cm/cm
Melt Flow 5.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
cm³/10 min Volumetric Rate; ISO 1133
 5.0 - 17 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 74 - 79ASTM D2240
Tensile Strength at Break 37.9 - 55.2 MPaASTM D638
Tensile Strength, Yield 34.5 - 55.2 MPaASTM D638
Elongation at Break <= 20 %ASTM D638
Elongation at Yield <= 4.0 %ASTM D638
Tensile Modulus 3100 - 5170 MPaASTM D638
Flexural Strength 138 - 207 MPa
@Strain 5.0 %
ASTM D790
Flexural Modulus 5520 - 6890 MPaASTM D790
Compressive Strength 138 - 172 MPaASTM D695
Izod Impact, Notched 40.0 - 80.1 J/mASTM D256
Izod Impact, Unnotched 267 - 534 J/mASTM D256
Coefficient of Friction, Dynamic 0.12vs. steel; ASTM D1894
Coefficient of Friction, Static 0.18vs. steel; ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+11 ohm-cm
 1.00e+13 ohm-cmDry; IEC 60093
Dielectric Constant 28.8 - 33.5
@Frequency 1000 Hz
ASTM D150
 33
@Frequency 100 Hz
Dry; IEC 60250
Dissipation Factor 0.061
@Frequency 100 Hz
Dry; IEC 60250
 0.060 - 0.080
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 36.0 - 45.0 µm/m-°CASTM D696
CTE, linear, Parallel to Flow 40.0 µm/m-°CDry; ISO 11359-1/-2
Melting Point 165 - 170 °CASTM D3418
 170 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 132 - 149 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 - 127 °CASTM D648
 120 °CDry; ISO 75-1/-2
Glass Transition Temp, Tg -40.0 °C10°C/min; Dry; ISO 11357-1/-2
 -40.6 - -38.3 °CASTM D7028
Decomposition Temperature 375 °C1% wt. loss, TGA, in air
 410 °C1% wt. loss, TGA, in nitrogen
Flammability, UL94 V-0IEC 60695-11-10
 V-0
@Thickness 0.800 mm
IEC 60695-11-10
Oxygen Index 44 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 °CCompression Molding; Molding Temperature; ISO 293
Melt Temperature 230 °CInjection Molding; ISO 294
 200 - 270 °C
Mold Temperature 90.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
Compression Molding Demolding Temperature (°C)40ISO 293
Form as DeliveredPellets
Moisture SensitiveNo
Processing MethodsInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding
Arkema KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Arkema KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema Kynar® 720 Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion

PARKG901 / 144526

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.