Single component permanently conductive clear acrylic coating which provides effective static elimination for electronics safe handling area and explosive atmosphere applications. Fully compliant with BS EN 61340- 5.1:2007 and ATEX. Contains carbon nanotubes, a graphene derivative. Application in lighting, windows, clear covers and lids, displays etc.Information provided by TBA Protective Solutions |