MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omnia Plastica Omniamid PA6 GHR HR - Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it is more shock resistant and self-lubricating. It is also easier to machine and U.V. ray resistance is better than that of natural Omniamid.

Features:

  • Wear resistance: better than natural PA6
  • Tensile stress and compressive strength: same as Omniamid G, whilst the shock resistance is higher, the fatigue resistance is more elevated.
  • Self-lubricating: the friction coefficient is low
  • Ageing resistance: weatherproof and good resistance at low temperature
  • Black colour
Weak Point:

It is hygroscopic even if to a lower extent than natural PA6G. Because of the molecular structure, large-sized cast pieces have better quality than those of small dimensions.

Application:

  • Mechanical: thanks to its good mechanical features and the possibility to obtain large-sized pieces, this material is mainly used to produce large diameter gears, pulleys, wheels and anti-wear guides. Due to the excellent abrasion resistance it is used in the building of parts for construction machines, excavators and earthmovers to produce gear wheels, guide bearings, bearings, sliding bearings etc. In the shipbuilding industry its improved weather resistance makes it suitable for rollers, haulage, sliding guides, bearings. In cable-car systems its uses include pulleys, wheels and sliding blocks.
  • Food contact: it cannot be used in contact with food.
  • Electrical: usage in the electrical field is to be avoided as the electrical properties change with the change in moisture content. It is sometimes used when its mechanical features are requested.
  • Chemical: it is resistant to alkali, inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO.1183 DIN.53479
Moisture Absorption at Equilibrium 2.2 %50% relative humidity
Water Absorption at Saturation 6.0 %23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 88dry sample; ISO2039.2
Ball Indentation Hardness 170 MPaISO2039.1 DIN.53456
Tensile Strength at Break 90.0 MPaISO.527 DIN.53455
Elongation at Break 20 %ISO.527 DIN.53455
Tensile Modulus 3.50 GPaISO.527 DIN.53455
Compressive Strength 20.0 MPa1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 0.500 J/cm²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.40on dry ground steel; load =0.05MPa; speed =0.6 m/s
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmISO.93 DIN.53482
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 30.0 kV/mmISO.243 DIN.53481
Dissipation Factor 0.050
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.280 W/m-KDIN.52612
Melting Point 220 °C
Maximum Service Temperature, Air 100 °CContinuous; 5000 hours based on a tensile stress of 50% at 23° C.
 160 °Cshort period, no load
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °CISO.75 DIN.53461
Minimum Service Temperature, Air -30.0 °Cimpact conditions and heavy loads not considered
Flammability, UL94 HB
Oxygen Index 25 %ISO.4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POMNIA12 / 55609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.