MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BYK Gelwhite® H Bentonite
Categories: Ceramic; Clay

Material Notes: Gelwhite® H is a highly purified white Bentonite manufactured from carefully selected, extremely pure ore deposits. Gelwhite® H exhibits low acid demand and interacts with both inorganic and organic cations. In formulations that requires tightly controlled rheology and reduced syneresis or that are acidic in pH, Gelwhite® H is ideally suited.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brightness 80 - 82 %80 - 82 %GE Brightness
Particle Mesh Size 200 Mesh200 MeshWet, 0%
pH 9.5 - 10.59.5 - 10.5
 
Component Elements PropertiesMetricEnglishComments
Al2O3 14.48 %14.48 %
CaO 1.73 %1.73 %
Fe2O3 1.36 %1.36 %
H2O, Water 5.0 - 8.0 %5.0 - 8.0 %
MgO 3.08 %3.08 %
Na2O 3.37 %3.37 %
SiO2 59.4 %59.4 %
TiO2 0.208 %0.208 %
 
Descriptive Properties
Color/FormFine Powder
Swelling>24 mls

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Gelwhite® L Bentonite
BYK Gelwhite® GP Bentonite
BYK Laponite® D Magnesium Silicate
BYK Laponite® B Fluorosilicate
BYK Gelwhite® LS Rheology Modifier

PBYK055 / 185052

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.