MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ex-Tech Plastics PerformaTech™ PVC Ex-Alloy 200 Reprocessed Vinyl
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Ex-Tech Plastics has long been a market leader in reprocessing vinyl sheet used for a variety of high quality thermoformed packaging. From retail packaging to tri-folds to trays to blister and clamshell packaging.

Characteristics:
Superior utility grade
Clear, standard and custom colors
Tear resistant

End Uses:
Retail packaging
Blister packaging
Clamshells
Tri-folds
Trays

Information provided by Ex-Tech Plastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 46.2 MPa6700 psiASTM D638
Elongation at Break >= 100 %>= 100 %ASTM D638
Modulus of Elasticity 2.07 GPa300 ksiASTM D638
Izod Impact, Notched 1.44 J/cm2.70 ft-lb/inSOP-MEC-002.01
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 62.0 °C144 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 85 %85 %Gardner 20°
 
Descriptive Properties
AppearanceBlue Tint
Cold Impact-35°CASTM D1790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Chlorinated PVC (CPVC)
High-leaded brass, UNS C34200, OSO35 Temper flat products
GEHR Plastics PVC-U Polyvinylchloride
ExxonMobil Escorene™ FL 01418 Ethylene Vinyl Acetate Copolymer (European Grade)
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 50 Gauge

PEXTEC995 / 133220

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.