Varcum 29346 is a two-stage, powdered phenolic resin containing hexamethylenetetramine as a curing agent. APPLICATION: General purpose bonded abrasives. FEATURES: - Medium condensation resin.
- Excellent performance in medium and medium-high density wheels.
- Can be used in cold-pressed snagging wheels, centerless grinding wheels and general purpose cut-off wheels.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |