MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Glastic T-160 Fiberglass-Reinforced Polyester Laminate
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical loading and moderately high temperature. NEMA grade GPO-1.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 g/ccASTM D-792
Water Absorption 0.30 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 14000 psiASTM D-638
Flexural Strength 29000 psiASTM D-790
 25000 psi
@Temperature 130 °C
ASTM D-790
Compressive Strength 56000 psiASTM D-695
Adhesive Bond Strength 1790 psiASTM D-229
Izod Impact, Notched 12.0 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 16.2 kV/mmPerpendicular in Oil; ASTM D-149
 19.6 kV/mmPerpendicular in Air; ASTM D-149
Arc Resistance 140 secASTM D-495
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
 
Descriptive Properties
Electric Strength kV, ASTM D14915Parallel 48/50
 40Parallel as rec`d
Standard ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate
Röchling Glastic Laminates/Shapes UTS Fiberglass-Reinforced Polyester Laminate
Röchling Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod
Röchling Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod
Röchling Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester

PGLASW0 / 41934

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.