Resin Type: Homopolymer Characteristics: Excellent Clarity, Good Impact Strength, Good Sealability, Low Slip Applications:Food Packaging, Case Shrink Wrap, Laminations Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical. |