  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton ARC 855N Ceramic-Filled Epoxy Industrial Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 100% solids, reinforced thin film coating to protect structures against chemical, abrasion, and corrosion. ARC 855N industrial coating is designed to:
  • Meet the requirements of Mil Spec 32171
  • Protect metal against abrasion, corrosion and chemical attack
  • Provide extended wear and predictable maintenance
  • Apply by brush or roller

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³Cured
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Tensile Strength at Break 23.4 MPa3400 psiASTM D638
Flexural Strength 55.2 MPa8000 psiASTM D790
Compressive Strength 82.7 MPa12000 psiASTM D695
Adhesive Bond Strength 34.6 MPa5020 psiPull-Off Adhesion; ASTM D4541
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C26.0 µin/in-°FASTM C531
Maximum Service Temperature, Air 65.0 °C149 °FWet Service
 120 °C248 °FDry Service
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month
@Temperature 10.0 - 32.0 °C
24.0 Month
@Temperature 50.0 - 89.6 °F
Dry, Unopened Containers
 
Descriptive Properties
Cathodic DisbondmentPasses 60 DaysASTM G8
ColorBlue or gray
Salt FogNo Rust >10,000 hrsASTM B117
Vertical Sag Resistance,No Sag21°C (70°F) and 375 µm (15 mil)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS039n / 239854

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.