MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sax Polymers SAXALEN PPH325GK20 Polypropylene Homopolymer, 20% Glass Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: SAXALEN PPH325GK20 is a 10% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. It has a increased stiffness and a optimized warpage grade.

Information provided by SAX Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
from MVR; ISO 1033
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 46.0 MPa6670 psi5 mm/min; ISO 527-1
Elongation at Break 4.0 %4.0 %5 mm/min; ISO 527-1
Tensile Modulus 3.00 GPa435 ksi1 mm/min; ISO 527-1
Flexural Strength 79.0 MPa11500 psi2 mm/min; ISO 178
Flexural Modulus 2.70 GPa392 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  15.0 kJ/m²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1U
 29.0 kJ/m²
@Temperature 23.0 °C
13.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 3.60 J/cm²
@Temperature 23.0 °C
17.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °F80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 125 °C257 °FB/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 250 °C428 - 482 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled
Sax Polymers SAXALEN PPH303G20 Polypropylene Homopolymer, 20% Glass Filled

PSAXP924 / 150873

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.