MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® HTN51G45HSL BK083 PA6T/XT-GF45
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: 45% Glass Reinforced, PPA, High Performance Polyamide

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccDAM; ISO 1183
Water Absorption 3.6 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.00 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmDAM; ISO 294-4, 2577
 0.0020 cm/cmannealed; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cmDAM; ISO 294-4, 2577
 0.0070 cm/cmannealed; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 230 MPa50% RH; ISO 527-1/-2
 240 MPaDAM; ISO 527-1/-2
Elongation at Break 2.0 %50% RH; ISO 527-1/-2
 2.3 %DAM; ISO 527-1/-2
Tensile Modulus 15000 MPaDAM; ISO 527-1/-2
 15500 MPa50% RH; ISO 527-1/-2
Flexural Modulus 13200 MPaDAM; ISO 178
Poissons Ratio 0.3350% RH
 0.33DAM
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µm/m-°CDAM; ISO 11359-1/-2
 14.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 15.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°CDAM; ISO 11359-1/-2
 45.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 69.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Melting Point 300 °Cfirst heat; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 285 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 265 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 95.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 135 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.850 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 29.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 325 °COptimum, Injection
 320 - 330 °CRange, Injection
Mold Temperature 150 °COptimum, Injection
 140 - 180 °CInjection; higher temperature needed for thinner sections
Drying Temperature 100 °CInjection
Dry Time 6.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6T/XT,GF45,M1CGHR,S10-140
Part Marking Code>PA6T/XT-GF45<ISO 11469
 >PPA-GF45<SAE J1344
PolymerPA6T/XT-GF45
Resin IdentificationPA6T/XT-GF45ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® HTN51G45HSL NC010 PA6T/XT-GF45
AISI Type P20 Mold Steel (UNS T51620)
Celanese Zytel® HTNFE8200 NC010 PA6T/XT-HI
Aluminum 7075-O
Celanese Zytel® 70G50HSLA BK039B PA66-GF50

PDSX5438 / 198078

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.